One Step Microcrystalline Glass Preparation Using Smelting Slag from
2 days agoThe slag was dried at 105 °C for 12 h after water cooling some of the microcrystalline glass obtained after drying was taken crushed and ground into a fine powder and regular shaped blocks of microcrystalline glass were taken and finely ground with an agate mortar and sieved through No 200 mesh to obtain a fine powder